ITEM项目 |
18s |
20s |
22S |
|
Line Density 线密度(D-TEX) |
325 |
293 |
265 |
|
Break Elongation Rate 断裂伸长率(Min)% |
230 |
230 |
230 |
|
Asymmetry Rate on Break Elongation断裂伸长不匀率(Max)% |
7 |
7 |
7 |
|
Break Strength断裂强力(cN)(Min) |
280 |
270 |
265 |
|
Asymmetry Rate on Break Strength断裂强力不匀率(Max)% |
7 |
7 |
7 |
|
Break Elongation Rate After Dipped浸胶后断裂伸长率(Min)% |
160 |
160 |
160 |
|
Asymmetry Rate on Break ElongationAfter Dipped浸胶后断裂伸长不匀率(Max)% |
8 |
8 |
8 |
|
Break Strength After Dipped浸胶后断裂强力(cN) (Min) |
270 |
270 |
250 |
|
Asymmetry Rate on Break Strength After Dipped 浸胶后 断 裂强力不匀率(Max)% |
8 |
8 |
8 |